Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 80.7 MPa | 11700 psi | Short Beam, Dry, RT, 0° Direction; ASTM D2344 |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Shear Strength | 80.7 MPa | 11700 psi | Transverse; ASTM D732 |
Greene Tweed Arlon® 1163 PEEK, Glass Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |