Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.586 MPa | 85.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 1/4-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 3/8-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | >= 0.586 MPa | >= 85.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRH-10 - 1/8- 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | >= 0.586 MPa | >= 85.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRH-10 - 3/16 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-49 - 1/4 - 2.1 Woven Kevlar Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-49 is manufactured using KEVLAR® 49 fabric. A thermosetting adhesive is used for the node bonds and a 350°F cure modified epoxy resin i.. |
|||
Shear Strength | >= 0.586 MPa | >= 85.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRP - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP/F35 - 2.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 1/4-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 3/16-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 0.586 MPa | >= 85.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR III 3/8-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | >= 0.586 MPa | >= 85.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | >= 0.586 MPa | >= 85.0 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRH-10 - 1/4 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Shear Strength | 0.586 MPa @Temperature 107 °C, Time 1.81e+6 sec |
85.0 psi @Temperature 225 °F, Time 504 hour |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Shear Strength | 0.586 MPa | 85.0 psi | |
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Shear Strength | 0.586 MPa @Temperature 107 °C, Time 1.81e+6 sec |
85.0 psi @Temperature 225 °F, Time 504 hour |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |