Polymer Property : Secant Modulus, MD = 0.120 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.120 GPa
17.4 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film
The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti..
Secant Modulus, MD 0.120 GPa
17.4 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight
The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac..
Secant Modulus, MD 0.120 GPa
17.4 ksi
ASTM D882
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process..
Secant Modulus, MD 0.120 GPa
17.4 ksi
ASTM D882
Eastman 5220 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good bubble stability, Medium coefficient of friction, Excellent low temperature properties, Good heat seal characteristicsApplica..
Secant Modulus, MD 0.120 GPa
17.4 ksi
ASTM D882
Eastman 5222 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good low temperature properties, Good heat seal characteristics, High slip, High antiblock, Good optical propertiesApplications:Ic..
Secant Modulus, MD 0.120 GPa
17.4 ksi
ASTM D882
Eastman 5223 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good heat seal characteristics, High antiblock, No Slip, Good processability. Slip 0 ppm. Antiblock 5000 ppm.Applications:Ice ba..
Secant Modulus, MD 0.120 GPa
17.4 ksi
ASTM D882
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze..
Secant Modulus, MD 0.120 GPa
17.4 ksi
2% Secant Modulus; ASTM-D882
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene
TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all..
Secant Modulus, MD 0.120 GPa
17.4 ksi
2% Secant Modulus; ASTM-D882
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene
TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness..
Secant Modulus, MD 0.120 GPa
17.4 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film
The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc..