Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.5171 GPa | 75.00 ksi | 2% Secant; ASTM D882 |
Dow Saran® 18L-WP White Plastic Barrier Film Saran™ 18L-WP is a white biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow |