Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, TD = 0.193 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.193 GPa
28.0 ksi
0.01; ASTM D882
Eastman 184MF Polyethylene Film  (discontinued **)
Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character..
Secant Modulus, TD 0.193 GPa
28.0 ksi
1% Secant; ASTM D882
Eastman 1840F Polyethylene  (discontinued **)
Polyethylene 1840F is a low-density formulation with no slip or antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is characterized by..
Secant Modulus, TD 0.193 GPa
28.0 ksi
1% Secant; ASTM D882
Eastman E6838-899F Polyethylene  (discontinued **)
E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr..
Secant Modulus, TD 0.193 GPa
28.0 ksi
1% Secant; ASTM D882
Eastman E6838-923F Polyethylene  (discontinued **)
E6838-923F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarit..
Secant Modulus, TD 0.193 GPa
28.0 ksi
1% Secant; ASTM D882
Eastman E6838-997F Polyethylene  (discontinued **)
E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
LyondellBasell Montell 12C01G2 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
LyondellBasell Montell 12C01G3 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: ..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
LyondellBasell Montell 12C01G4 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
LyondellBasell Montell 12C01G5 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
LyondellBasell Montell 16501F3 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
LyondellBasell Montell 16501F4 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
LyondellBasell Montell 16501F6 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets ..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
LyondellBasell Montell 16501F7 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
LyondellBasell Montell 16501F8 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee..
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
Huntsman PE 1253 EVA Film Extrusion  (discontinued **)
2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to..
Copyright © lookpolymers.com All Rights Reserved