Polymer Property : Secant Modulus, TD = 0.4826 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.4826 GPa
70.00 ksi
2% Secant; ASTM D882
Dow Saran® 18L-WP White Plastic Barrier Film
Saran™ 18L-WP is a white biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow