Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.117 GPa | 17.0 ksi | ASTM D882 |
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o.. |
|||
Secant Modulus, TD | 0.117 GPa | 17.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-318 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Secant Modulus, TD | 0.117 GPa | 17.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-319 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Secant Modulus, TD | 0.117 GPa | 17.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light.. |
|||
Secant Modulus, TD | 0.117 GPa | 17.0 ksi | ASTM D882 |
Huntsman PE1605 EVA Film Extrusion
(discontinued **) 6% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Secant Modulus, TD | 0.117 GPa | 17.0 ksi | ASTM D882 |
Huntsman Rexell® L3103 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent optics and sealability with good toughnessApplications: Stretch wrap and coextruded film for general packaging.FD.. |