Heat Seal Strength Initiation Temperature 120 °C
248 °F
2 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow ELITE™ 5110G Enhanced Polyethylene Resin
™ 5110G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of high modulus and excellent impact strength, allowing for down gauging in bag applicatio..
Heat Seal Strength Initiation Temperature 120 - 200 °C
248 - 392 °F
DuPont Teijin Films Melinex® CORE 2 Polyester Film
Melinex® CORE 2 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well..
Heat Seal Strength Initiation Temperature 120 °C
248 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe..
Heat Seal Strength Initiation Temperature 120 °C
248 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin General Purpose Resin Excellent Strength Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, de..
Heat Seal Strength Initiation Temperature 120 °C
248 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe..
Heat Seal Strength Initiation Temperature 120 °C
248 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f..
Heat Seal Strength Initiation Temperature 120 °C
248 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe..
Heat Seal Strength Initiation Temperature 120 °C
248 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th..
Heat Seal Strength Initiation Temperature 120 °C
248 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe..
Heat Seal Strength Initiation Temperature 120 °C
248 °F
TOTAL Method
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin  (Unverified Data**)
Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p..