Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 120 °C | 248 °F | 2 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow ELITE™ 5110G Enhanced Polyethylene Resin ™ 5110G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of high modulus and excellent impact strength, allowing for down gauging in bag applicatio.. |
|||
Heat Seal Strength Initiation Temperature | 120 - 200 °C | 248 - 392 °F | |
DuPont Teijin Films Melinex® CORE 2 Polyester Film Melinex® CORE 2 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well.. |
|||
Heat Seal Strength Initiation Temperature | 120 °C | 248 °F | 1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Heat Seal Strength Initiation Temperature | 120 °C | 248 °F | 1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin General Purpose Resin Excellent Strength Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, de.. |
|||
Heat Seal Strength Initiation Temperature | 120 °C | 248 °F | 1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Heat Seal Strength Initiation Temperature | 120 °C | 248 °F | 1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f.. |
|||
Heat Seal Strength Initiation Temperature | 120 °C | 248 °F | 1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Heat Seal Strength Initiation Temperature | 120 °C | 248 °F | 1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th.. |
|||
Heat Seal Strength Initiation Temperature | 120 °C | 248 °F | 1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Heat Seal Strength Initiation Temperature | 120 °C | 248 °F | TOTAL Method |
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**) Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p.. |