Mechanical Properties Metric English Comments
Tenacity >= 0.140 N/tex
>= 1.59 g/denier
SGL Carbon Group PANOX® FA C063 EEA High performance Crimped staple oxidized textile fiber, For carbon/carbon and spinning
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Tenacity >= 0.140 N/tex
>= 1.59 g/denier
SGL Carbon Group PANOX® FA C063 SSC High performance Crimped staple oxidized textile fiber, For felts and non-wovens
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Tenacity >= 0.140 N/tex
>= 1.59 g/denier
SGL Carbon Group PANOX® FA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments
For carbon/carbon and spinning. PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not b..
Tenacity >= 0.140 N/tex
>= 1.59 g/denier
SGL Carbon Group PANOX® SA C063 EEA High performance oxidized textile fiber, Crimped staple fiber, For carbon/carbon and spinning
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Tenacity >= 0.140 N/tex
>= 1.59 g/denier
SGL Carbon Group PANOX® SA C063 SSC High performance oxidized textile fiber, Crimped staple fiber, For felts and non-wovens
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Tenacity >= 0.140 N/tex
>= 1.59 g/denier
SGL Carbon Group PANOX® SA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments
For carbon/carbon and spinning. PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not b..