Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 379 MPa @Temperature 650 °C, Time 360000 sec |
55000 psi @Temperature 1200 °F, Time 100 hour |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |