Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 90.0 MPa @Temperature 927 °C, Time 360000 sec |
13100 psi @Temperature 1700 °F, Time 100 hour |
Plate |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Rupture Strength | 90.0 MPa @Temperature 870 °C, Time 360000 sec |
13100 psi @Temperature 1600 °F, Time 100 hour |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |