Polymer Property : Flexural Modulus = 2.30 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.30 GPa

@Temperature -20.0 °C
334 ksi

@Temperature -4.00 °F
ISO 178
Polykemi AB POLYfill PPHC K3020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus 2.30 GPa

@Temperature 23.0 °C
334 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612  (Unverified Data**)
Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Flexural Modulus 2.30 GPa

@Temperature 23.0 °C
334 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.1%); ASTM-D790
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.30 GPa

@Temperature 80.0 °C
334 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.30 GPa

@Temperature -40.0 °C
334 ksi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.9%); ASTM-D790
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.30 GPa

@Temperature 163 °C
334 ksi

@Temperature 325 °F
Hexcel® HexPly® 954-3 Curing Cyanate Resin
HexPly® 954-3 is a 350°F (177°C) curing cyanate resin with excellent resistance to moisture absorption, outgassing and microcracking. HexPly® 954-3 is formulated for autoclave or press molding u..
Flexural Modulus 2.30 GPa

@Temperature 163 °C
334 ksi

@Temperature 325 °F
Wet (Immersion at 170°F for 7 days)
Hexcel® HexPly® 954-2A Curing Cyanate Resin
HexPly® 954-2A is a 350°F (177°C) curing toughened cyanate resin with low moisture absorption, and excellent microcracking resistance. HexPly® 954-2A is formulated for autoclave or press molding..
Flexural Modulus 2.30 GPa

@Temperature 250 °C
334 ksi

@Temperature 482 °F
EN ISO 178
Ensinger TECASINT™ 2011 Polyimide (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Flexural Modulus 2.30 GPa

@Temperature 23.0 °C
334 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6  (Unverified Data**)
Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Flexural Modulus 2.30 GPa

@Temperature -20.0 °C
334 ksi

@Temperature -4.00 °F
ISO 178
Polykemi AB POLYfill PPHC K5020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus 2.30 GPa

@Temperature -20.0 °C
334 ksi

@Temperature -4.00 °F
ISO 178
Polykemi AB POLYfill PPHC K8020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus 2.30 GPa

@Temperature -20.0 °C
334 ksi

@Temperature -4.00 °F
ISO 178
Polykemi AB POLYfill PPHC K9020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB