Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 3.00 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.00 GPa

@Temperature -40.0 °C
435 ksi

@Temperature -40.0 °F
ASTM D790
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Flexural Modulus 3.00 GPa

@Temperature 23.0 °C
435 ksi

@Temperature 73.4 °F
Hexcel® HexPly® 954-3 Curing Cyanate Resin
HexPly® 954-3 is a 350°F (177°C) curing cyanate resin with excellent resistance to moisture absorption, outgassing and microcracking. HexPly® 954-3 is formulated for autoclave or press molding u..
Flexural Modulus 3.00 GPa

@Temperature 23.0 °C
435 ksi

@Temperature 73.4 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin
HexPly® 954-2A is a 350°F (177°C) curing toughened cyanate resin with low moisture absorption, and excellent microcracking resistance. HexPly® 954-2A is formulated for autoclave or press molding..
Flexural Modulus 3.00 GPa

@Temperature 23.0 °C
435 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PP HBK1501515 Polypropylene, Multifiller High Gloss
Information provided by Polykemi AB
Flexural Modulus 3.00 GPa

@Temperature 150 °C
435 ksi

@Temperature 302 °F
ISO 178
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
Copyright © lookpolymers.com All Rights Reserved