Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.908 J/cm

@Thickness 12.7 mm
1.70 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP310E Cotton Fabric
Description: Manufactured with a domestic cotton fabric and phenolic resin. Similar to NP310 with improved moisture resistance and electrical properties. Mechanical properties equivalent to NP310. M..
Izod Impact, Unnotched 0.908 J/cm

@Thickness 12.7 mm
1.70 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP313 Cotton Fabric
Description: Canvas phenolic laminate with molybdenum disulfide lubricant. Mechanical properties slightly lower than NP310.Thickness Tested: 0.062", 0.125" & 0.500"
Izod Impact, Unnotched 0.908 J/cm

@Thickness 12.7 mm
1.70 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP315 Cotton Fabric
Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should ..
Izod Impact, Unnotched 0.908 J/cm

@Thickness 12.7 mm
1.70 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP320 Cotton Fabric
Description: Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than NP310. For smaller and more intricate shape..
Izod Impact, Unnotched 0.908 J/cm

@Thickness 12.7 mm
1.70 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP342 Cotton Fabric
Description: Fine weave canvas phenolic material with fabric construction weight intermediate to NP310 and NP320. Designed for better machining than grade NP310 and lower cost than NP320.Thickness T..
Izod Impact, Unnotched 0.908 J/cm

@Thickness 12.7 mm
1.70 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP344 Cotton Fabric
Description: Fine weave canvas laminate with high temperature phenolic resin and molybdenum disulfide lubricant. Good machining properties and low coefficient of thermal expansion. Better machining ..
Izod Impact, Unnotched 0.908 J/cm

@Thickness 12.7 mm
1.70 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP424 Laminate
Description: Composite material composed of woven glass fabric surfaces and paper core combined with epoxy resin. Primarily used in the printed circuit board industry. Easy punching and excellent el..
Izod Impact, Unnotched 0.910 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.70 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Izod Impact, Unnotched 0.910 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.70 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.