Mechanical Properties Metric English Comments
Flexural Modulus 0.0450 GPa
6.53 ksi
ISO 178
Polimeri Europa Clearflex® MQ F0 Very Low Density Polyethylene
Clearflex MQ F0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati..
Flexural Modulus 0.0450 GPa

@Temperature 49.0 °C
6.53 ksi

@Temperature 120 °F
ASTM D790
DuPont Elvax® 750 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.0450 GPa
6.53 ksi
ISO 178
Chengdu Polyster FH3303 Thermoplastic Polyether-ester Elastomer (TPEE)
Blend of H3303 and self-made flame retardant material. Excellent flex resistance at low temperatures. Excellent flex-fatigue resistance. Applications requiring flexibility at low temperatures and fl..
Flexural Modulus 0.0450 GPa
6.53 ksi
ISO 178
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Flexural Modulus 0.0450 GPa
6.53 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® MV 3000 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 3000 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
Flexural Modulus 0.0450 GPa
6.53 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 3000 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
Flexural Modulus 0.0450 GPa
6.53 ksi
ASTM D790
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Flexural Modulus 0.0450 GPa
6.53 ksi
ASTM D638
Arkema Group LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 5500 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. These grade is characterised by a high fluidity. Functional group..
Flexural Modulus 0.0450 - 0.115 GPa
6.53 - 16.7 ksi
Average value: 0.0733 GPa Grade Count:3
Overview of materials for Very Low Density Polyethylene (VLDPE)
This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va..
Flexural Modulus 0.0450 GPa
6.53 ksi
ASTM D638
Arkema Group LOTRYL® 17 BA 04 Copolymer Ethylene - Butyl Acrylate
LOTRYL® 17 BA 04 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 17 BA 04 is used as tie layer in coextrusion PP/PE, for extrusi..