Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0900 GPa | 13.1 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Flex® TPO D-6510 Data provided by Multibase. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | ISO 178 |
Polimeri Europa Greenflex® ML 30 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion Greenflex ML 30 is an ethylene vinyl acetate copolymer (EVA) for injection molding and profile extrusion. Items produced with Greenflex ML 30 show good ESCR and elasticity.Main Applications: Green.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | ISO 178 |
Polimeri Europa Greenflex® ML 31 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion Greenflex ML 31 is an ethylene vinyl acetate copolymer (EVA) for injection molding applications and extrusion profile. Greenflex ML 31 contains additive waxes to obtain high production speed.Main A.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | ISO 178 |
Polimeri Europa Greenflex® MP 34 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding Greenflex MP 34 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MP 34 combines high fluidity with high elasticity.Main Applications: Gree.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | ASTM D790 |
Rotuba MS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD801A PPE-TPE Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD801A PPE-TPE (Asia Pacific) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD801A PPE-TPE (Europe-Africa-Middle East) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE (Europe-Africa-Middle East) Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE (Europe-Africa-Middle East) Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE (Asia Pacific) Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE (Asia Pacific) Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | ASTM D790 |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | ISO 178 |
Chengdu Polyster H4543 Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and injection grade. Contains improved color- stable antioxidants. Applications requiring high original color retention. Molded and injected products for consumer use, such as se.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | ISO 178 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur.. |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | |
Arkema Group Pebax® MV 1074 Polyether Block Amide (PEBA) Typical application: Breathable filmInformation provided by Arkema Group |
|||
Flexural Modulus | 0.0900 GPa | 13.1 ksi | ISO 178; ASTM D790 |
Arkema Group Pebax® MV1074 Polyether Block Amide |