Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D790 |
SABIC MG200024 Linear Low Density Polyethylene for Compounding Product Description: MG200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding. It is in the powder form designed to give g.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D790 |
SABIC MG500026 Linear Low Density Polyethylene for Compounding Product Description: MG500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding applications. It is in the powder form and h.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ISO 178 |
Polimeri Europa Riblene® MP 30 R Low Density Polyethylene - Injection Molding Riblene MP 30 R is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MP 30 R are characterized by a medium rigidity.Main Applications: Riblene MP 30 R is suitable for in.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ISO 178 |
Polimeri Europa Riblene® MP 31 Low Density Polyethylene - Injection Molding Riblene MP 31 is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.Parts made by Riblene MP 31 are characterized by a medium rigidity.Main Applications: Riblene MP 31 i.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ISO 178 |
Polimeri Europa Riblene® MP 31 R Low Density Polyethylene - Injection Molding Riblene MP 31 R is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.Parts made by Riblene MP 31 R are characterized by a medium rigidity.Main Applications: Riblene MP .. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D790 |
Quadrant EPP Proteus® LDPE - Low Density Polyethylene (ASTM Product Data Sheet) |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D790 |
SABIC M200024 Linear Low Density Polyethylene for Injection Molding Product Description: M200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give good f.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D790 |
SABIC M500026 Linear Low Density Polyethylene for Injection Molding Product Description: M500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excell.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 800A Polyethylene
(discontinued **) Polyethylene 800A is a general-purpose low density formulation used for injection molding applications that require good stress-crack resistance. Polyethylene 800E is used in general-purpose extrus.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 800E Polyethylene
(discontinued **) Polyethylene 800E is used in general-purpose extrusion applications that also require good stress resistance. This formula complies with FDA regulations at 21 CFR177.1520 (c)(2.2) for use in articl.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman Voridian 800P Polyethylene
(discontinued **) General purpose low density formulation used for extrusion coating applications that require good stress resistance. This formula complies with FDA regulations at 21 CFR 177.1520(c)(2.1) for use i.. |
|||
Flexural Modulus | 0.200 - 5.50 GPa | 29.0 - 798 ksi | Average value: 2.20 GPa Grade Count:88 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D760-66 |
Micropol L20 Low density polyethylene rotational molding powder Has a high gloss finish, and outstanding toughness. Information provided by Micropol Limited |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D760-66 |
Micropol L7 Low density polyethylene rotational molding powder Has a high gloss finish, and outstanding toughness. Information provided by Micropol Limited |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ISO 178 |
Solvay TECHNYL® B 230 PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP YP003 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YP003 is a compound based on Polyester Elastomer containing PTFE, Silicone. Added features include; Internally Lubricated. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon FX99030 PE (Europe-Africa-Middle East) LNP * Stat-kon* FX99030 is a compound based on Polyethylene resin containing Carbon Powder. Added features include: Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-M.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8010 Availability: North AmericaForms: PelletsProcessing Method: Extrusion Blow Molding and Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2644 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled for auto application |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ISO 178 |
Ecomass® 1002ZC85 Stainless Steel Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.Stainless Steel Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Pol.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | Tangent, 16:1 span:depth,0.5in/min; ASTM D790 |
Chevron Phillips Marlex® 1003 LDPE Injection Molding Resin Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: HousewaresTamper evident, snap-on capsWine bottle sleeve capsInfo.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | Tangent, 16:1 span:depth,0.5in/min; ASTM D790 |
Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: Large housewaresTamper evident, snap-on capsFeminine hygiene appl.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® LT 4060 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® LT 4060 Polyamide Alloy Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | ASTM D790 |
Buckeye Polymers BP Flex A9008 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 2mm/min; ASTM D790 |
3M Dyneon™ PVDF 32008/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 32008/0009 is an ultra-flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 32008/0009 also has a very low brittleness te.. |
|||
Flexural Modulus | 0.200 GPa | 29.0 ksi | 2mm/min; ASTM D790 |
3M Dyneon™ PVDF 32008/0000 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesInformation provided by Dyneon, A 3M.. |