Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.290 - 12.9 GPa | 42.1 - 1880 ksi | Average value: 2.60 GPa Grade Count:723 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ASTM D790 |
ExxonMobil Iotek® 8610 Sodium Ionomer
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low melt index sodium ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact stre.. |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant. |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific) LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications. |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ASTM D790 |
Sterigenics Raprex® R-300 Branched Linear Low Density Polyethylene Applications: Foam and ExtrusionRAPREX® R-300 is a linear low density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique .. |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ASTM D790 |
Sterigenics Raprex® R300D Branched Linear Low Density Polyethylene Applications: Foam and ExtrusionRAPREX® R300D is a linear low density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique .. |
|||
Flexural Modulus | 0.290 GPa | 42.0 ksi | ASTM D 790 |
Teknor Apex APEX® 02-A0310A-107 Polyvinyl Chloride, Semi-Rigid Notes: 80°C Insulation; RoHS Compliant Uses: Automotive Electronics; InsulationWire Types: GPTAgency Ratings: SAE J1128 Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor .. |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ASTM D790 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ASTM D790 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ASTM D790 |
Toyobo PELPRENE™ S2004FS Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ISO 178 |
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.290 GPa | 42.1 ksi | ASTM D790 |
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Flexural Modulus | 0.290 GPa | 42.0 ksi | ASTM D790 |
Aaron Industries AAROLENE® ARPE LD 300-1 Low Density Polyethylene Compounded Resin AAROLENE® ARPE 300 Series Polyethylene Compounded Resin LDPEColor may be specified. Melt Flow Index may be specified. Specific Gravity may be specified. |