Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.379 GPa | 55.0 ksi | ASTM D790 |
M. Holland Company LL700 LLDPE
(discontinued **) Features: High ESCR (Stress Crack Resist.), Good Flexibility, High FlowUses: Closures, Household GoodsProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Flexural Modulus | 0.379 GPa | 55.0 ksi | Tangent, 0.05 in/min; ASTM D790 |
LyondellBasell Hifaxâ„¢ CA138A Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA138A low modulus thermoplastic olefin (TPO) resin is designed for impact modification and injection molding applications. It is based on material produced from Basell'.. |
|||
Flexural Modulus | 0.379 GPa | 55.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Flexural Modulus | 0.379 GPa | 55.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-1000-105UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Flexural Modulus | 0.379 GPa | 55.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-94-T1422A-100 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Flexural Modulus | 0.379 GPa | 55.0 ksi | ASTM D790 |
Lubrizol Estane® ALR CL65D Thermoplastic Polyurethane Type: Estane® ALR CL650 is an aliphatic, polycaprolactone-based TPU with a Shore D Durometer of 65.Features: Contains a UV package that enhances outdoor weatherability. This high performance resin.. |
|||
Flexural Modulus | 0.379 - 0.7198 GPa | 55.0 - 104.4 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D0850 BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Flexural Modulus | 0.379 GPa | 55.0 ksi | Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790 |
Phillips Sumika Marlex® CHP-055 Thermoplastic Polyolefin
(discontinued **) Applications: Passenger-side Air--bag coverSoft interior trimInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product ha.. |