Mechanical Properties Metric English Comments
Flexural Modulus 0.390 GPa
56.6 ksi
ASTM D790
NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin  (discontinued **)
Molded Plaque Properties. Features: high flow.Applications: general purpose, housewares.Data provided by the manufacturer.
Flexural Modulus 0.390 GPa

@Temperature 90.0 °C
56.6 ksi

@Temperature 194 °F
ASTM D790
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic  (discontinued **)
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Flexural Modulus 0.390 GPa
56.6 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCA901 PPE-TPE
Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL..
Flexural Modulus 0.390 GPa
56.6 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCA901 PPE-TPE
Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL..
Flexural Modulus 0.390 GPa
56.6 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific)
Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL..
Flexural Modulus 0.390 GPa
56.6 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific)
Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL..
Flexural Modulus 0.390 GPa
56.6 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Europe-Africa-Middle East)
Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL..
Flexural Modulus 0.390 GPa
56.6 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Europe-Africa-Middle East)
Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL..
Flexural Modulus 0.390 GPa
56.6 ksi
ASTM D790
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Flexural Modulus 0.390 GPa
56.6 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Flexural Modulus 0.390 GPa
56.6 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Flexural Modulus 0.390 GPa
56.6 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® 7033 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Flexural Modulus 0.390 GPa
56.6 ksi
ASTM D790
Ashley Polymers Ashlene® 734-SP5 Nylon 6, Flexible Grade
A highly flexible grade of Nylon 6 with outstanding impact.Data provided by the manufacturer
Flexural Modulus 0.390 GPa
56.6 ksi
ASTM D790
Ashley Polymers Ashlene® TD930H Nylon 12
A plasticized Nylon 12 offering outstanding flexibility with superior moisture and chemical resistance, UV and heat stabilized for weatherability.Data provided by the manufacturer
Flexural Modulus 0.390 GPa
56.6 ksi
ASTM D790
Ashley Polymers Ashlene® LT940H Nylon 11
An economy grade, general purpose, highly flexible, natural Nylon 11 resin with UV stabilizers.Data provided by the manufacturer