Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.407 GPa | 59.0 ksi | 2% secant; ASTM D790 |
ExxonMobil LL 6202.19 Injection Molding Resin Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Flexural Modulus | 0.407 GPa | 59.0 ksi | 2% Secant; ASTM D638 |
ExxonMobil LLDPE LL 6201.19 Linear Low Density Polyethylene Resin Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Flexural Modulus | 0.407 GPa | 59.0 ksi | 2% Secant; ASTM D638 |
ExxonMobil LLDPE LL 6202.19 Linear Low Density Polyethylene Resin Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |