Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.480 GPa | 69.6 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE G 7890 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.480 GPa | 69.6 ksi | ASTM D790 |
Polymer Industries Densetec LDPE Sheet Polymer Industries Densetec LDPE is a material that`s soft, flexible, and tough, even at low temperatures. Because of the fact that Densetec LDPE has very good formability traits and is very pliable.. |
|||
Flexural Modulus | 0.480 GPa | 69.6 ksi | ASTM D790 |
NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin Molded Plaque Properties. Features: High flow, Granular, Improved dispersion concentrates.Applications: housewares, additive and color, masterbatches/compounding.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.480 GPa | 69.6 ksi | ASTM D790 |
Reliance Industries Reclair R35042 Reclair R35042 is a medium density polyethylene grade designed for the rotomoulding process. It exhibits good toughness and environmental stress resistance.Information provided by Reliance Industri.. |
|||
Flexural Modulus | 0.480 GPa | 69.6 ksi | ASTM D790 |
Reliance Industries Reclair R35042 Polyethylene Rotational molding Medium Density Polyethylene grade. Characteristics:good toughness, good impact resistance, good environmental stress crack resistance. Applications:chemical tanks, water storage .. |
|||
Flexural Modulus | 0.480 - 0.970 GPa | 69.6 - 141 ksi | Average value: 0.767 GPa Grade Count:21 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Flexural Modulus | 0.480 GPa | 69.6 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ ETA-5081 Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convoluted .. |
|||
Flexural Modulus | 0.480 GPa | 69.6 ksi | ASTM D790 |
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
Flexural Modulus | 0.480 GPa | 69.6 ksi | Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced Low density linear polyethylene. This low density, linear resin is tailored for blow molded containers that require: Excellent processabilityExcellent ESCRApplications: Typical blow molded applica.. |
|||
Flexural Modulus | 0.480 GPa | 69.6 ksi | Tangent, 16:1 span:depth,0.5in/min; ASTM D790 |
Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRBroad fusion rangeExcellent melt strengthGood processabilityExcellent flexibilityImproved output and texturingApplications: Coextruded ca.. |
|||
Flexural Modulus | 0.480 GPa | 69.6 ksi | ISO 178 |
BASF Ultramid® HFX 33 PA6 (Dry) Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |