Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.552 - 30.0 GPa | 80.0 - 4350 ksi | Average value: 16.1 GPa Grade Count:29 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Flexural Modulus | 0.552 - 25.5 GPa | 80.0 - 3700 ksi | Average value: 14.4 GPa Grade Count:18 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
Multibase Multi-Flamâ„¢ 2103 HDPE Polyethylene Features:Flame RetardantHalogen Content, Low to NoneBlooming, None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
Techmer ES Electrablend® PPS 06001 Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer DescriptionPolytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. ApplicationTPP 608 is designed specifically for automotive fascia.. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer DescriptionPolytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. ApplicationTPP 608 is designed specifically for automotive fascia.. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer DescriptionPolytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. ApplicationTPP 608 is designed specifically for automotive fascia.. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
Lubrizol ESTALOC® 60155 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Flexural Modulus | 0.552 GPa | 80.1 ksi | |
CMW® ELKONITE® 50S Infiltrated Tungsten Silver contact material ASTM B631, Class C, infiltrated For arcing and current carrying electrical contacts.Information provided by CMW Inc. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.552 GPa | 80.1 ksi | Procedure A; ASTM D790 |
Solvay Engineered Polymers DEXFLEX® E160 TPO
(discontinued **) Description: DEXFLEX® E160 thermoplastic olefinic elastomer (TPO) is designed for extrusion applications that require thermal stability, excellent low-temperature properties, and good dimensional s.. |
|||
Flexural Modulus | 0.552 GPa | 80.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |