Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.630 GPa | 91.4 ksi | ASTM D790 |
3M Dyneon™ PFA 6525N Perfluoroalkoxy Fluorothermoplastic
(discontinued **) The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra.. |
|||
Flexural Modulus | 0.630 GPa | 91.4 ksi | ASTM D790 |
LG Chemical LUPOL TE-5005H Thermoplastic Elastomer Alloy, Dimensional Stability LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Flexural Modulus | 0.630 GPa | 91.4 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Flexural Modulus | 0.630 GPa | 91.4 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific) LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Flexural Modulus | 0.630 GPa | 91.4 ksi | ASTM D790 |
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Flexural Modulus | 0.630 GPa | 91.4 ksi | ASTM D790 |
Asahi Glass Fluon® P-63P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Flexural Modulus | 0.630 GPa | 91.4 ksi | ASTM D790 |
Asahi Glass Fluon® P-810UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Flexural Modulus | 0.630 - 1.60 GPa | 91.4 - 232 ksi | Average value: 1.33 GPa Grade Count:10 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |