Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.650 GPa | 94.3 ksi | |
Plastcom SLOVALEN EQ 18 N PP, basic type FeaturesModified PE with special heat and processional stabilization. Application in extrusion of profiles and pipes, blowing of bottles and jerrycans. Delivered in black colour.Packaging, transport.. |
|||
Flexural Modulus | 0.650 GPa @Temperature 23.0 °C |
94.3 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYelast TPE EC90 D50 P05B Thermoplastic Elastomer, PP/EPDM Information provided by Polykemi AB |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D790 |
Petromont 7000 Medium Density Polyethylene Resin Petromont HDPE 7000 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is readily processed by blown sheet or flat die extrusi.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ISO 178 |
Total Lacqtene® 2006 TN 35 HDPE pipe coating
(discontinued **) LACQTENE® 2006 TN 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 TN 35 may be used for pipe and sheet extrusion (flex.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D790 |
NOVA Chemicals Sclair® 8504 UV8D, 8504G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.650 - 14.1 GPa | 94.3 - 2050 ksi | Average value: 7.23 GPa Grade Count:127 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 110-1327 LMDPE Rotational Molding Resin Description: ICORENE 110-1327 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1327 LMDPE Rotational Molding Resin Description: ICORENE 115-1327 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 190-1327 LMDPE Rotational Molding Resin Description: ICORENE 190-1327 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | 2mm/min; ASTM D790 |
Kingfa PA6-MG30 30% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D760-66 |
Micropol Microlin ML53 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Adsylâ„¢ 5C30F Thermoplastic Olefin Resin Primary Processing Method: Film extrusionKey Features: thermoplastic olefin resins for film extrusion, good clarity and gloss, good moisture barrier properties, very low seal initiation temperature,.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Adsylâ„¢ 5C37F Thermoplastic Olefin Resin Primary Processing Method: Film extrusionKey Features: thermoplastic olefin resins for film extrusion, good clarity and gloss, good moisture barrier properties, very low seal initiation temperature,.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D790 |
Iran Petrochemical (PCC) 3840 UA Medium Density Polyethylene MD3840UA is a linear medium density polyethylene (MDPE) with butene copolymer. This polymer has good impact strength, excellent external and internal surface finish, whiteness, good stress cracking .. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Asia Pacific) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Europe-Africa-Middle East) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 3840 UA MDPE Rotational Molding Applications:Rotational items: tanks, containers, etc...Injection molded technical parts and closureInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (S.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ M3504DXP Octene (C8) Rotational Molding Resin Natural base resin available in powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tanks, spray t.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ M70 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cyc.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ M735 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cycle.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ISO 178 |
Borealis Borclear™ RB709CF Polypropylene Ethylene Copolymer Borclear™ RB709CF is a propylene -ethylene copolymer. This grade is suitable for the manufacturing of unoriented film on blown film lines. Applications: Borclear™ RB709CF is recommended for seal.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® LE 60 LM Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ISO 178 |
Total Finacene® BM359SG HDPE, blow molding
(Unverified Data**) FINACENE® BM359 SG has been especially designed for the manufacture of blow moulded bottles (up to 5 liters) with a superior surface gloss and contact transparency. It is recommended either in mono.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D790 |
Petromont 7001 Medium Density Polyethylene Resin Petromont HDPE 7001 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ISO 178 |
Polyplastic Armlen® PE MF 70-2FR Magnesium Hydroxide Filled Polyethylene 70% Magnesium HydroxideFor extrusion of fire resistant aluminum composite panels.Information provided by PolyPlastic Group. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D790 |
SCG Chemicals EL-Lene™ M50 Octene (C8) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tan.. |
|||
Flexural Modulus | 0.650 GPa | 94.3 ksi | ASTM D790 |
Petromont 7002 Medium Density Polyethylene Resin Petromont HDPE 7002 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi.. |