Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D790 |
Rochling Engineered Plastics Polystone® G HDPE Extruded Sheet Information provided by Röchling Engineered Plastics. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 25-0110 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 2% Secant-Method 1; ASTM D790 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D 790 |
Total CD 4300 HDPE extrusion Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D790 |
Total HDPE 7194 High Density Polyethylene, Specialty Extrusion Resin Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationUSP Class VI compliantApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformat.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D790 |
Total HDPE 7195 High Density Polyethylene, Specialty Extrusion Resin Characteristics:Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformation pr.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 0.05 in/min; ISO 178 |
CTC X-PRO CTC PP 5002 Polypropylene Copolymer X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI6120Q4 High Impact Copolymer Polypropylene Description: Extra High Izod Impact, Superior Low Temperature Drop Impact, Good Paint AdhesionApplications: Suggested Uses Include Compounding, Automotive, Injection MoldingThis resin meets the requ.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI6200Q4 High impact Copolymer Polypropylene Description: Extra high izod impact, superior low temperature drop impact, good paint adhesion. Applications: Suggested uses include toys, video cassettes, compounding. Process: Compounding. This r.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D 790 |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |