Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products P251-00 Polypropylene Copolymer, Natural Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | >= 1.03 GPa | >= 150 ksi | ASTM D790 |
S&E Specialty Polymers GPP1005HF Series PP Application: UL94 V-2, Flame-retardant polypropylene compounds for injection molding applications.Information provided by S&E Specialty Polymers |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 25-2102 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyMirae Moplen EP300L Injection Molding Grade Polypropylene Moplen EP300L is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300L is a block copolymer selected by customers for use in in.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR750CL-02 Polypropylene, Random Copolymer, NX-8000 based COPYLENE™ CR750CL-02 is an easy molding, high melt flow random copolymer that has good see-through and contact clarity in injection molding applications and is formulated with advanced technology. .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 1% Secant; ASTM D 790 |
Chevron Phillips Marlex® 9506H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: superior physical properties, medium molecular weight distribution, wide range of processing conditions, low parison sag, excellent stress crack resistan.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Ravago Manufacturing Americas Echo® RPPC 20/6 BK Polypropylene Copolymer Available in North America Recycled Content: Yes Features: CopolymerColor: Black Form: Pellets Information provided by Ravago |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 1% Secant, 0.05 in/min; ASTM D790 |
LyondellBasell Pro-faxâ„¢ SG899 Polypropylene Copolymer Description: Pro-faxâ„¢ SG899 high flow, high impact polypropylene copolymer resin is tailored for use in automotive interior head impact applications. This resin is designed to be run in convent.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 9450 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF30 L N BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
A. Schulman PP 1817-01 Polypropylene Utility Grade Random Co-Polymer DescriptionPolypropylene PP 1817-01 is a utility grade random co-polymer which can be used for general purpose injection molding, extrusion, or blow molding applications. It does not have a gel spe.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | |
TriStar TriSteel AC Metal Backed PTFE Bearing System Ultraflon 601 (AC) POM lined metal backed bearing system, boundary lubrication required, high PV. Ultraflon 601 POM Liner is a lubricant enhanced acetal material for use in lubricated or unlubricate.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | |
TriStar TriSteel AT Metal Backed PTFE Bearing System Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
ExxonMobil HDPE BU46-055 High Density Polyethylene Resin Product Description: BU46-055 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt .. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Clariant 6008 L Nylon 6, High Impact, Injection Molding Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 1% Secant; ASTM D790 |
ExxonMobil HDP8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Secant @ 1% strain; ASTM D-790 |
Bapolene® PP5021 Polypropylene, Blow Molding Grade Bapolene PP5021 is a PP Random Copolymer designed for blow molding and extrusion applications. This resin exhibits excellent clarity, impact strength, stiffness and processability. This product me.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D-790 |
Axiall 3802 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
Flexural Modulus | 1.03 - 1.72 GPa | 150 - 250 ksi | ASTM D790 |
Alcoa KAMA 3202 Freezer Modified High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableColors availa.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Flexural Modulus | 1.03 - 3.10 GPa | 149 - 450 ksi | Average value: 1.89 GPa Grade Count:27 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
SCG Chemicals EL-Lene™ H5211PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE80 pipe, non pressure pipesCertification: Certified by LNEI.. |