Mechanical Properties Metric English Comments
Flexural Modulus 1.48 GPa
215 ksi
Method I (3 point load), Procedure B); ASTM D790
Multibase Nylex™ 2185 CR Polyamide + PP
Forms: PelletsFeatures:Chemical Resistance, GoodInformation provided by Multibase
Flexural Modulus 1.48 GPa
215 ksi
1% Secant; ASTM D790
ExxonMobil HD 9856BA Blow Molding Resin  (discontinued **)
HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracki..
Flexural Modulus 1.48 GPa
215 ksi
0.05 in/mm, 1% Secant, Procedure A; ASTM D790
Phillips 66 COPYLENE® CH350 Polypropylene Homopolymer
COPYLENE™ CH350 is a controlled rheology, barefoot homopolymer designed for application as a base resin for compounding, consumer products and other injection molding applications.Applications: Inj..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790A
BP Amoco Innovene 1088 Polypropylene Homopolymer  (discontinued **)
Suggested fabrication methods: ExtrusionFeatures: General purposeTypical applications: Water quenched blown filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fr..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790A
Ineos H13G-00 Polypropylene Homopolymer  (discontinued **)
Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790A
BP Amoco Amoco® 7644 Polypropylene Homopolymer  (discontinued **)
Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property ..
Flexural Modulus 1.48 GPa
215 ksi
Tangent; ASTM D790
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Flexural Modulus 1.48 GPa
215 ksi
1% Secant; ASTM D790
Flint Hills P4C6Z-059 Homopolymer Polypropylene
Homopolymer, UL certified, and FDA compliant.Features: Controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills Res..
Flexural Modulus 1.48 GPa
215 ksi
1% Secant; ASTM D790
Flint Hills P4G4Z-011 Homopolymer Polypropylene
Homopolymer, UL certified, USP Class VI certified, and FDA compliant.Features: Applications: Injection molding: general purpose, extruded decorative ribbon, and extruded fiber.Former Huntsman polypr..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790A
Ineos H05A-00 Polypropylene Homopolymer
Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified ..
Flexural Modulus 1.48 GPa
215 ksi
1% Secant, 0.05 in/min; ASTM D790A
Ineos H12G-01 Polypropylene Homopolymer
Grade H12G-01 is a general purpose homopolymer. This material meets the requirements of the US Food and Drug Administration as specified in 21 CFR 177.1520 for use in food-contact applications for f..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790A
Ineos Innovene H07B-00 Polypropylene Homopolymer
Extrusion. Features: No Slip, Antiblock.Applications: Cast filmTypical property data below from injection molded samples.
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790
Iran Petrochemical (PCC) 60505 High Density Polyethylene
60505 is a HDPE injection molding grade which combines high stiffness with good physical properties. This resin is well suited for crates and toys applications.Application: crates, injection molding..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790
LyondellBasell Petrothene® LB832001 High Density Polyethylene
ApplicationsPETROTHENE LB 8320-00 resin is designed for sheet extrusion, vacuum forming and thermoforming. This resin exhibits very low sag, high stiffness.Regulatory StatusLB 8320-00 meets the req..
Flexural Modulus 1.48 GPa
215 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP
LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE...
Flexural Modulus 1.48 GPa
215 ksi
ASTM Test
Styrolution Styrolux 3G33 SBC
Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and ..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790
Styrolution Styrolux® GH 62 SBC
Description: Styrolux® GH 62 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warp..
Flexural Modulus 1.48 GPa
215 ksi
Tangent; ASTM D790
Plastics Group Polifil® RMC-10 10% Calcium Carbonate-Reinforced Polypropylene, High Impact
Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin..
Flexural Modulus 1.48 GPa
215 ksi
Tangent; ASTM D790
Washington Penn Homopolymer Polypropylene
Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array ..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790A
CPC - Vycom PROTEC® Copolymer Polypropylene (CPP)
Protec CP is one of various types of "impact copolymers"—a rapidly growing segment of the thermoplastic sheet market. In contrast to homopolymer polypropylene (which involves the polymerization of ..
Flexural Modulus 1.48 GPa
215 ksi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
ExxonMobil Paxon™ AD60-005 Blow Molding Resin
Product Description: AD60-005 is a medium molecular weight districution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
Flexural Modulus 1.48 GPa
215 ksi
Tangent; ASTM D790
Chevron Phillips Marlex® 9519H High Density Polyethylene, Blow Molding
This gas phase, high molecular weight, homopolymer with antistatic agent is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt strength..
Flexural Modulus 1.48 GPa
215 ksi
ASTM Test
BASF Styroclear GH 62 SBC
Styroclear GH 62 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790
NOVA Chemicals Novapol® HB-W558-A HDPE Extrusion Resin  (discontinued **)
Molded Plaque Properties. Features: High molecular weight, excellent impact strength, high rigidity, easy processing.Applications: large part blow molding, large oil drums.Data provided by the manu..
Flexural Modulus 1.48 GPa
215 ksi
ISO 178
Polyram RamLloy PVB702 Nylon/ABS Alloy, Impact Modified
Impact modified, UV stabilized Nylon/ABS alloy for injection molding applications.Information provided by Polyram.
Flexural Modulus 1.48 GPa

@Temperature 23.0 °C
215 ksi

@Temperature 73.4 °F
ASTM D790A
Ineos H12G-00 Polypropylene Homopolymer
This is a general purpose homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsG..
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790A
Ineos H14A-00 Polypropylene Homopolymer
Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,..
Flexural Modulus 1.48 GPa

@Temperature 23.0 °C
215 ksi

@Temperature 73.4 °F
1% Secant; ASTM D790A
Ineos H20E-00 Polypropylene Homopolymer
This is a homopolymer containing antistatic designed for injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Application..
Flexural Modulus 1.48 GPa
215 ksi
Tangent; ASTM D790
Chevron Phillips Marlex® 9518H High Density Polyethylene, Blow Molding
This gas phase, high molecular weight, homopolymer is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt strengthAre durable and recycl..