Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Flexural Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP CIQ15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 1.50 - 2.50 GPa | 218 - 363 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Modulus | >= 1.50 GPa | >= 218 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 2062T (62107) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM D790 |
Shell Carilon® DA6P2L10 Polyketone, High Performance Lubricated Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6P2L10 is a high-performance lubricated injection molding grade with mechanical properties which .. |
|||
Flexural Modulus | >= 1.50 GPa | >= 218 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1552N (YF39S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Total Finathene® 6002 HDPE, blow molding, pipe
(discontinued **) FINATHENE® 6002 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 6002 has been especially developed for the manufacturing of toys and of b.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Iran Petrochemical (PCC) Moplen EP-S31HP Polypropylene Moplen EP-S31HP is a heterophasic polypropylene copolymer with an exceptional mechanical properties balance. In comparison with standard polypropylene copolymers with the same fluidity, Moplen EP-.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM D790 |
Iran Petrochemical (PCC) Moplen Z 30 G Polypropylene Moplen Z 30 G is a high flow homopolymer for injection molding and compounding applications. Moplen Z 30 G exhibits a high stiffness and an outstanding processability for shorter cycle times and eas.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Lucite International Diakon® ST45G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ TRA-3263EC/1 Thermoplastic Olefin Resin Key Features: fractional melt flow, high modulus, extrusion grade thermoplastic olefin resin, high flexural modulus, high impact strength, good surface appearance, excellent processabilityApplicatio.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ TRC704D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TRC704D medium high melt flow, 1,500 MPa flexural modulus, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and proce.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 5 mm/min; GOST 9550 |
Sibur H030 GP/1 Polypropylene Homopolymer General purpose product, is used in injection molding, extrusion and thermal molding applications. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp FF001 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FF001 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM Test |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX1180 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1180 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Borealis HD822CF Polypropylene HD822CF is a polypropylene homopolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Total PPH 5069 Polypropylene Homopolymer, Fiber Polypropylene PPH 5069 is a homopolymer polypropylene with a Melt Flow index of 6 g/10 min.Polypropylene PPH 5069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 527-2 |
Total PPH 7059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7059 is homopolymer.ApplicationATOFINA Polypropylene PPH 7059 is intended for extrusion of staple fibers for non-woven applications. It exhibits excellent spinning propert.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 60 g/10 min.Polypropylene PPC 11642 is characterized by high fluidity with good mechanical prope.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM-D790 |
Polyram RamOfin PPC501 Polypropylene, Flame Retardant Flame retardant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
ExxonMobil PP1055E2 Polypropylene Homopolymer Product Description: A nucleated homopolymer resin with good flowability and antistatic properties. It is designed for molding of media packaging, containers and other articles requiring fast moldi.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 2 mm/min; ISO 178 |
Eurostar Starglas FF001 HDPE, Glass Fiber Filled Starglas FF001 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM D790 |
Carmel Olefins CAPILENE® Y 50 V Polypropylene Homopolymer CAPILENE® Y 50 V is an ultra high melt flow rate polypropylene homopolymer suitable for thin walled injection molding and as a base resin for compounds applications. The product combines high stiff.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Cathay PA512 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, Conditioned Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM Test |
BASF Styroclear GH 58 SBC Styroclear GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Unipetrol PP MONSTEN® FC 110 Polypropylene Homopolymer Applications include injection molding, packaging films, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |