Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.725 GPa | 250.2 ksi | ASTM D790 |
Petromont 1100 High Density Polyethylene Resin Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b.. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | ASTM D790 |
Total PPH 3740WR Polypropylene, High Flow Nucleated Homopolymer Injection Molding Easy Flow TOTAL Polypropylene 3740WR exhibits exceptionally easy flow characteristics.FDA. 3740WR complies with all applicable FDA and USDA regulations and may be used under these provisions for .. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.725 GPa | 250.2 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |