Mechanical Properties Metric English Comments
Flexural Modulus 1.91 GPa
277 ksi
ASTM D790
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
Flexural Modulus 1.91 GPa
277 ksi
13 mm/min; ASTM D790
PolyOne Geon™ L4605 Green 5765 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid)
Information provided by PolyOne
Flexural Modulus 1.91 - 8.27 GPa
277 - 1200 ksi
Average value: 2.54 GPa Grade Count:66
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Flexural Modulus 1.91 GPa

@Thickness 6.40 mm
277 ksi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUPOL HF5157Z PP+Rubber+MF, High Flow and Stiffness, High Impact
Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good PaintabilityApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provided by LG Chemical
Flexural Modulus 1.91 GPa

@Thickness 3.20 mm
277 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY MP5000AM PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Flexural Modulus 1.91 GPa
277 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp IP003 PA6.12
LNP* Lubricomp* IP003 is a Nylon 6/12 base resin containing PTFE and Silicone.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 1.91 GPa
277 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Flexural Modulus 1.91 GPa
277 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP VN001 Super Tough Nylon
LNP* LUBRICOMP* VN001 is a compound based on Super Tough Nylon containing 2% MOS2. Added feature of th is grade is: Wear Resistant.
Flexural Modulus 1.91 GPa
277 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent
Information provided by Samsung Cheil Industries.
Flexural Modulus 1.91 GPa
277 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced
Material with superior chemical resistance that can be used in the interior/exterior material of household appliances that require heat resistanceInformation provided by Samsung Cheil Industries.
Flexural Modulus 1.91 GPa
277 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade
Information provided by Samsung Cheil Industries.
Flexural Modulus 1.91 GPa
277 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced
Material with superior chemical resistance that can be used in the interior/exterior material of household appliances that require heat resistanceInformation provided by Samsung Cheil Industries.
Flexural Modulus 1.91 GPa
277 ksi
ASTM D790
Samyang Trirex® 3000H Polycarbonate, Low-temperature Impact
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3000H is a low temperature impact grade.Applications: Mobile Phone Housing, high gloss..
Flexural Modulus 1.91 GPa
277 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT
4.2 specific gravity, PBT, gray
Flexural Modulus 1.91 GPa
277 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
Flexural Modulus 1.91 GPa

@Thickness 3.20 mm
277 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 6530 Antistatic Polystyrene
Characteristics Prevents dust patterns due to static charges Eliminates need of coatings Fully colorable Processing Injection molding Extrusion & Forming Applications Meter housings Foodservice ..
Flexural Modulus 1.91 GPa
277 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent
Information provided by Samsung Cheil Industries.
Flexural Modulus 1.91 GPa
277 ksi
ASTM D790
Westlake Plastics HIPS High Impact Polystyrene, Compression Molded
Compression molded HIPS is a low cost plastic material that is easily machined and fabricated. It is frequently used for preproduction prototyping. HIPS is a FDA compliant use in food processing a..
Flexural Modulus 1.91 GPa
277 ksi
Zylog Hipolyene® 1533 NM Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.91 GPa
277 ksi
Zylog Hipolyene® 6251 Y M2 Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.91 GPa
277 ksi
Zylog Hipolyene® 8501 T6 B Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.91 GPa
277 ksi
ASTM D790
Westlake Plastics HIPS High Impact Polystyrene
HIPS is a low cost plastic material that is easy to machine and fabricate. It is often specified for low strength structural applications when impact resistance, machinability, and low cost are req..
Flexural Modulus 1.91 GPa

@Thickness 6.40 mm
277 ksi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Flexural Modulus 1.91 GPa

@Thickness 6.40 mm
277 ksi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Flexural Modulus 1.91 GPa

@Thickness 6.40 mm
277 ksi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Flexural Modulus 1.91 GPa

@Thickness 6.40 mm
277 ksi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Flexural Modulus 1.91 GPa
277 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade
Information provided by Samsung Cheil Industries.