Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.0 GPa | 1450 ksi | STN EN ISO 178 |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
Premix Premi-Glas® 2103-22 CRSX Polyester BMC Premi-Glas® 2103-22 CR-SX is a 22% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
Premix Premi-Glas® 2103-22 CR-SX-HT Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-22 CR-SX-HT is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL .. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | DIN 53452 |
Qualchem Danamid FCF-20 Polyamide 6, 20% Carbon Fiber Reinforced with carbon fiber, antistatic and conductive.Information provided by Qualchem Zrt. |
|||
Flexural Modulus | 10.0 - 13.0 GPa | 1450 - 1890 ksi | Compression; ISO 178 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Flexural Modulus | 10.0 - 24.0 GPa | 1450 - 3480 ksi | Average value: 16.8 GPa Grade Count:14 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Flexural Modulus | 10.0 - 26.0 GPa | 1450 - 3770 ksi | Average value: 13.3 GPa Grade Count:8 |
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim.. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Flexural Modulus | 10.0 GPa @Temperature 22.0 °C |
1450 ksi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Flexural Modulus | 10.0 GPa @Temperature 22.0 °C |
1450 ksi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
Kuraray Genestarâ„¢ G1350H Nylon, 35% Glass Filled Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in .. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | |
Haysite Ultratrac® H950 Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) This new generation of high performance material meets or exceeds all requirements for NEMA GPO-2 or GPO-3. ULTRATRAC ® H950 is recognized by U.L. as a 94V-0 material and offers greater arc and t.. |
|||
Flexural Modulus | 10.0 GPa @Temperature 22.0 °C |
1450 ksi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Flexural Modulus | 10.0 GPa @Temperature 22.0 °C |
1450 ksi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® BMC 2800 Unsaturated Polyester UP BMC 2800 is a high performance BMC for matching the demands of medium and high voltage applications in the electrical field especially in respect of RTI 160+ according to Underwriters Laboratories .. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC003 PA 66 (Europe-Africa-Middle East) 15% carbon fibre reinforced Polyamide 66 injection moulding resin. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | ISO 178 |
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Flexural Modulus | 10.0 GPa | 1450 ksi | ISO 178 |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |