Mechanical Properties Metric English Comments
Flexural Modulus 8.00 - 10.0 GPa
1160 - 1450 ksi
Injection; ISO 178
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Flexural Modulus 8.00 - 10.0 GPa
1160 - 1450 ksi
Compression; ISO 178
Raschig Group 6501 DAIP
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Flexural Modulus 8.00 - 10.0 GPa
1160 - 1450 ksi
Compression; ISO 178
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Flexural Modulus 8.00 - 10.0 GPa
1160 - 1450 ksi
Injection; ISO 178
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
Flexural Modulus 5.00 - 10.0 GPa
725 - 1450 ksi
ASTM D790
Raschig Group PiMC 1221 High gloss
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Flexural Modulus 5.00 - 10.0 GPa
725 - 1450 ksi
ASTM D790
Raschig Group PiMC 1241 Sanitary, uni color
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Flexural Modulus 5.00 - 10.0 GPa
725 - 1450 ksi
ASTM D790
Raschig Group PiMC 1249 Sanitary, mix color
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Flexural Modulus 5.00 - 10.0 GPa
725 - 1450 ksi
ASTM D790
Raschig Group PiMC 1949 Granite colors
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Flexural Modulus 7.00 - 10.0 GPa
1020 - 1450 ksi
Injection; ISO 178
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Flexural Modulus 8.00 - 10.0 GPa
1160 - 1450 ksi
Injection; ISO 178
Raschig Group RALUPOL® 2200 UP Polyester
Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets..
Flexural Modulus 3.20 - 10.0 GPa
464 - 1450 ksi
Average value: 5.62 GPa Grade Count:178
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Flexural Modulus 4.14 - 10.0 GPa
600 - 1450 ksi
Average value: 7.29 GPa Grade Count:44
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Flexural Modulus 3.30 - 10.0 GPa
479 - 1450 ksi
Average value: 6.65 GPa Grade Count:11
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Flexural Modulus 7.00 - 10.0 GPa
1020 - 1450 ksi
DIN 53457
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated
Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH
Flexural Modulus 7.00 - 10.0 GPa
1020 - 1450 ksi
DIN 53457
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled
Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH
Flexural Modulus 8.00 - 10.0 GPa
1160 - 1450 ksi
ISO 178
Vyncolit 4221 XB Novolac Phenolic
Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group
Flexural Modulus 7.00 - 10.0 GPa
1020 - 1450 ksi
ASTM D790
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
Flexural Modulus 7.00 - 10.0 GPa
1020 - 1450 ksi
ASTM D790
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
Flexural Modulus 7.00 - 10.0 GPa
1020 - 1450 ksi
ASTM D790
Chang Chun Plastic PBT4130 Fire Retardant & 30% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
Flexural Modulus 0.228 - 10.0 GPa
33.0 - 1450 ksi
Average value: 2.35 GPa Grade Count:391
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Flexural Modulus 3.45 - 10.0 GPa
500 - 1450 ksi
Average value: 5.27 GPa Grade Count:18
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Flexural Modulus 3.00 - 10.0 GPa
435 - 1450 ksi
Average value: 5.60 GPa Grade Count:18
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..