Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.6 GPa | 1540 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th.. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific) LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 PPO LNP* STAT-KON* ZE0039 is a compound based on PPO resin containing 15% Carbon Fiber. Added features of this grade includes: Flame Retardant, Electrically Conductive. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 2X98703 ETFE LNP* THERMOCOMP* 2X98703 is a compound based on ETFE Copolymer resin containint Proprietary Filler(s). |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy .. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ASTM D790 |
Plenco 05118-T5 Phenolic, Granular, Compression Molded PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve.. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
Polyram PlusTek PA7001G7BK11 Nylon 66, 35% Glass Fiber Reinforced, Heat and UV Stabilized, Hydrolysis Resistant 35% Glass fiber reinforced, heat stabilized, UV stabilized, hydrolysis resistant Nylon 66. Approved by W.R.A.S.Information provided by Polyram. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178-93 |
Wellman Wellpet® MRGF102-BK1 PET, 35% Mineral/Glass Fiber Reinforced Typical data obtained from injection molded test bars, tested dry as molded at 73°F (23°C). Information provided by Wellman, Inc. Engineering Resins Division. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 462 Glass/Mineral Reinforced, PET Alloy, Impact Modified, UL Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 263 Glass Reinforced, Modified SMA Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXN PA 66 LNP* THERMOCOMP* RF007SXN is a Hydro-Stable, 35% Glass Fiber reinforced compound based on Nylon 66. Added features of this grade include: Heat Stabilized, NSF Listed. |
|||
Flexural Modulus | 10.6 GPa | 1540 ksi | ASTM D790 |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |