Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.7 GPa | 1550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
PolyOne LubriOne™ NJ-30CF/15T-2S Nylon 12
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ISO 178 |
Kuraray Genestarâ„¢ G1352A-M41 Nylon, 35% Glass Filled Low friction reinforced injection grade.Main Features:Low friction coefficientAbrasion resistanceExamples of applications:Friction and wear applicationGear and wheel |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 140 H2.0 DUS008 900051 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 40% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 C14 BK 14% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF30 FR BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 LE 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedInformation provided by TP C.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PPA GF30 HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC LNP* Thermocomp* Lexan_LGN5030 compound is a glass reinforced. Flame retardant. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedAppearance: BlackInformation.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM-D790 |
Polyram Polytron A30B02 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM-D790 |
Polyram Polytron A30N02 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam RF0023K PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023K is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding, Crosslinkable under Beta or Gamma RadiationInformation provided by Euros.. |