Polymer Property : Flexural Modulus = 1020 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.00 - 7.00 GPa
725 - 1020 ksi
Compression; ISO 178
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..