Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.752 GPa | 109 ksi | ASTM D790 |
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet) |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 HI HV TS PA6 with impact modifier PA 6 higher viscosity, heat stabilized, impact modified for extrusion and blow molding. Automotive applications as air ducts and fuel filter pipes, fuel and oil containers.Information Provided by Pl.. |
|||
Flexural Modulus | 0.750 GPa @Temperature 23.0 °C |
109 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYelast TPE R44 T10 Thermoplastic Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 0.750 - 7.60 GPa | 109 - 1100 ksi | Average value: 2.49 GPa Grade Count:236 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Modulus | 0.750 - 15.1685 GPa @Temperature 90.0 - 93.3 °C |
109 - 2200.03 ksi @Temperature 194 - 200 °F |
Average value: 7.96 GPa Grade Count:2 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 1% secant at 0.05 in/min; ASTM D790B |
LyondellBasell Montell 1900 UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferAp.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 1% secant at 0.05 in/min; ASTM D790B |
LyondellBasell Montell 1900CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of fraction, good chemical resistance, low odor and taste transfer, .. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 1% secant at 0.05 in/min; ASTM D790B |
LyondellBasell Montell 1900H UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, .. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 1% secant at 0.05 in/min; ASTM D790B |
LyondellBasell Montell HB312CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, .. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 1% secant at 0.05 in/min; ASTM D790B |
LyondellBasell Montell HB320CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, .. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 155-4060 LMDPE Rotational Molding Resin Description: ICORENE 155-4060 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 2mm/min; ASTM D790-86 |
Micropol Microcene MC122 Metallocene Based Polyethylene Rotational Molding Powder Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. .. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 2mm/min; ASTM D790-86 |
Micropol Microcene MC123 Metallocene Based Polyethylene Rotational Molding Powder Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. .. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 3840 EA MDPE Wire and Cable Grade Applications:Suitable for the production of silane cross-linkable compoundsLow voltage power cable insulationInjection molded technical parts and closureInformation provided by Interchim s.r.l., off.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Borealis Borseal™ TD120BF Terpolymer for BOPP Film Borseal TD120BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD120B.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Unipetrol PE HD LITEN® BB 10 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Unipetrol PE HD LITEN® FB 10 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Unipetrol PE HD LITEN® VL 20 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Polyplastics Duracon® TD-35 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Borealis Borseal™ TD220BF Terpolymer for BOPP Film Borseal TD220BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD220B.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | 0.05 in/min; ISO 178 |
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | SAE J949 |
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO Data |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Total Lacqtene® 2002 TN 40 HDPE, blow molding, pipe, sheet
(discontinued **) LACQTENE® 2002 TN 40 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer.Information provided provided by Total Petrochemicals.Total Petrochemic.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | |
Plastcom SLOVALEN PQ 53 N PP, imp. strength FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 66Z Nylon 66, Conditioned Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, Conditioned Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and.. |
|||
Flexural Modulus | 0.750 GPa | 109 ksi | ISO 178 |
Unipetrol PE HD LITEN® ZB 20 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |