Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D790 |
Rochling Engineered Plastics Polystone® G HDPE Extruded Sheet Information provided by Röchling Engineered Plastics. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 25-0110 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9301 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234360A; ASTM D 4976 Classification: PE 225, A 56607Applications:Base Resin for use in Gas, Oil Patch and Industrial Pipe.. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9302 HDPE Yellow Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607Applications:Natural Gas Distribution Piping and FittingsData provide.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 2% Secant-Method 1; ASTM D790 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 7040 G HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ISO 178 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ISO 178 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ISO 178 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP) LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ASTM D790 |
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6 26% crystallinity. Information supplied by Elastomer Engineering. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D 790 |
Total CD 4300 HDPE extrusion Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D790 |
Total HDPE 7194 High Density Polyethylene, Specialty Extrusion Resin Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationUSP Class VI compliantApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformat.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D790 |
Total HDPE 7195 High Density Polyethylene, Specialty Extrusion Resin Characteristics:Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformation pr.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 1% secant; ASTM D882 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 0.05 in/min; ISO 178 |
CTC X-PRO CTC PP 5002 Polypropylene Copolymer X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI6120Q4 High Impact Copolymer Polypropylene Description: Extra High Izod Impact, Superior Low Temperature Drop Impact, Good Paint AdhesionApplications: Suggested Uses Include Compounding, Automotive, Injection MoldingThis resin meets the requ.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI6200Q4 High impact Copolymer Polypropylene Description: Extra high izod impact, superior low temperature drop impact, good paint adhesion. Applications: Suggested uses include toys, video cassettes, compounding. Process: Compounding. This r.. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ASTM D790 |
Asahi Glass Fluon® AH-2000 LM-ETFE, Non-Conductive Type, Fluororesin Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive ag.. |
|||
Flexural Modulus | 0.793 GPa | 115 ksi | ASTM D 790 |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
LyondellBasell DEXFLEX® 810-1 TPO Description: DEXFLEX® 810-1 is a thermoplastic olefinic elastomer (TPO) that offers excellent weatherability, paintability and processability. DEXFLEX® 810-1 was designed to exceed the requiremen.. |