Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Plenco Valite 4100 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |
|||
Flexural Modulus | 8.24 GPa | 1190 ksi | 5 mm/min; ISO 178 |
Gromax BFG30-AH00B2 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.24 GPa | 1190 ksi | 5 mm/min; ISO 178 |
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. |
|||
Flexural Modulus | 8.21 GPa | 1190 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific) LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon WC003 PBT (Europe-Africa-Middle East) LNP* Stat-kon* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON WC003 PBT (Europe-Africa-Middle East) LNP* Stat-kon* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 8.24 GPa | 1190 ksi | |
Shinil Chemical SHINFLAME PBT GF Flame Retardant Polymer Lamp Housing SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF004 Acetal Copolymer LNP THERMOCOMP* KF004 is a compound based on Acetal Copolymer resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF0067K PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF0067K is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790, ISO 178 |
EPICHEM Epiter PBT GF 30 Polybutylene Terephthalate, 30% Glass Characteristics: 30% glass fibre filled |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
E-Polymers Tekaloy® T80GFR , Flame Retardant, 30% Glass Fiber Reinforced PBT/ABS Alloy 30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 8.22 GPa | 1190 ksi | ISO 178 |
Azdel AZMET® CM32350 35% continuous random fiber mat / PET resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polyethylene Terephthalate (PET) resin matrix. This composite material fea.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 610 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 283 PPO Alloy, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 284 PPO Alloy, Glass/Graphite Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass/Graphite Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 638 Nylon 6/6, Mineral Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO Value |
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he.. |
|||
Flexural Modulus | 8.20 GPa @Temperature 60.0 °C |
1190 ksi @Temperature 140 °F |
ASTM D790 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
PlastxWorld CEVIAN® B2506 30% GF PBT/ABS Alloy Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 8.21 GPa | 1190 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 LNP VERTON* PX00700 is a compound based on Nylon 6 resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Flexural Modulus | 8.21 GPa | 1190 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 (Asia Pacific) LNP* Verton* PX00700 is a compound based on Nylon 6 resin containing Long Glass Fiber. |