Mechanical Properties Metric English Comments
Flexural Modulus 12.3 GPa
1780 ksi
X, Y direction; Condition A; ASTM D790
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Flexural Modulus 12.3 GPa

@Temperature 23.0 °C
1780 ksi

@Temperature 73.4 °F
ISO 178
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Flexural Modulus 12.3 GPa
1780 ksi
ISO 178
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Flexural Modulus 12.3 GPa

@Temperature 23.0 °C
1780 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYshine PBT D201 FB52 PBT, Reinforced
Information provided by Polykemi AB
Flexural Modulus 12.3 GPa
1780 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN133G50 G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 12.3 GPa
1780 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66
LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant.
Flexural Modulus 12.3 GPa
1780 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* RE004 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 12.3 GPa
1780 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing Glass Fiber. Added features include: Easy Molding.
Flexural Modulus 12.3 GPa
1780 ksi
2 mm/min; ISO 178
Sax Polymers SAXAMID 226F10 Nylon 6.6, 50% Glass Fiber
SAXAMID 226F10 is a polyamide 6.6 injection-molding-grade reinforced with 50% glass fibers. It has high mechanical strength.Information provided by SAX Polymers
Flexural Modulus 12.3 GPa
1780 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Europe-Africa-Middle East)
LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 12.3 GPa
1780 ksi
ASTM D790
Plenco 08122 Polyester BMC, Compression Molded
PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..
Flexural Modulus 12.3 GPa
1780 ksi
ISO 178
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when..
Flexural Modulus 12.3 GPa
1780 ksi
ISO 178
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Flexural Modulus 12.3 GPa
1780 ksi
2.8mm/min; ASTM D790
Asia International Enterprise (Hong Kong) 60G8 Nylon 66, 40% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Flexural Modulus 12.3 GPa
1780 ksi
ASTM D790
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry  (discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..
Flexural Modulus 12.3 GPa
1780 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON ME006 PP
LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.