Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.850 GPa @Temperature 90.0 °C |
123 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Flexural Modulus | >= 0.850 GPa | >= 123 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4440R (40404) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 0.848 GPa | 123 ksi | 1% Secant; ASTM D790 |
Ravago Manufacturing Americas Echo® RPPC 20/10 BK Recycled Polypropylene Copolymer Polypropylene, Unreinforced, 20 MFI, 10 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT,.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | Secant; ASTM D3350 |
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid.. |
|||
Flexural Modulus | 0.850 GPa @Temperature 23.0 °C |
123 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPC 20000 Polypropylene Copolymer Information provided by Polykemi AB |
|||
Flexural Modulus | 0.850 GPa @Temperature 90.0 °C |
123 ksi @Temperature 194 °F |
ASTM D790 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Flexural Modulus | 0.850 - 0.850 GPa @Temperature 90.0 - 90.0 °C |
123 - 123 ksi @Temperature 194 - 194 °F |
Average value: 0.850 GPa Grade Count:1 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Flexural Modulus | 0.850 GPa @Temperature 23.0 °C |
123 ksi @Temperature 73.4 °F |
ISO 178 |
MBA Polymers PP 2182 Post-consumer recycled polypropylene copolymer Very high melt flow rate for injection molding application. Available in standard black.Information provided by MBA Polymers. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 3325M Polypropylene Random Copolymer CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD SEALABLE CONTAINS SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM EXTRUSION CPP FILM FOR LAMINATE , CPP FILM FOR PACKAGINGS |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | at 2 in/min; ASTM D790 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790/1 |
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important .. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ISO 178 |
Borealis Daploy™ WB260HMS Polypropylene Daploy™ WB260HMS is a propylene-based, structurally isomeric polymer. Applications: cushioning and protective packaging, door liners, lightweight packaging trays, beakers and containers, microwave.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | at 2 in/min; ASTM D790 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | at 2 in/min; ASTM D790 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | at 2 in/min; ASTM D790 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ISO 178 |
Borealis RD735CF Polypropylene Random Copolymer RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging .. |
|||
Flexural Modulus | 0.850 GPa @Temperature 23.0 °C |
123 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FN727 BK230A Nylon 6 Zytel® FN727 BK230A is a black, impact modified, plasticizer free, very flexible polyamide 6 alloy resin having good low temperature toughness, good heat aging and good chemical resistance. Uses in.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® LC6601 BK551 Nylon 612
(Unverified Data**) Plasticized Toughened Polyamide 612 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | 1% secant; ASTM D790 |
Braskem CP 195 Injection Molding Polypropylene Description: CP 195 is a very high melt flow rate heterophasic copolymer developed for high speed injection moulding machines and high productivity thin-walled injection moulded parts. The product f.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
Carmel Olefins CAPILENE® TR 50 Polypropylene Impact Copolymer Description: CAPILENE® TR 50 is a medium melt flow rate heterophasic copolymer with very high impact strength, even at low temperature, designed for injection molding. This grade combines good pr.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
Carmel Olefins CAPILENE® TT 75 AV Polypropylene Impact Copolymer Description: CAPILENE® TT 75 AV is a nucleated, controlled rheology heterophasic copolymer designed for injection molding. It is characterized by excellent impact strength, even at low temperatur.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
Carmel Olefins CAPILENE® TU 75 AV Polypropylene Impact Copolymer Description: CAPILENE® TU 75 AV is a high melt flow rate, controlled rheology heterophasic copolymer with very high impact strength, even at low temperature. It contains antistatic and nucleating.. |
|||
Flexural Modulus | 0.850 GPa @Temperature 93.0 °C |
123 ksi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2607-UV9 HDPE Injection Molding Resin
(discontinued **) Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | |
Total Lacqtene® 6002 FLG 42 HDPE film
(discontinued **) LACQTENE® 6002 FLG 42 is a medium density polyethylene resin with hexene as comonomer. This shows a broad molecular weight distribution ensuring outstanding processability. LACQTENE® 6002 FLG 42 h.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ISO 178 |
Polyplastic Armlen® PP 3IM Impact Modified Polypropylene Impact modified polypropylene composite materialInformation provided by PolyPlastic Group. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790/1 |
Borealis Borstar® HE6062 HDPE Black Jacketing Compound Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketin.. |