Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.90 GPa | 1290 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 35 Polyamide 6, 35% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 35% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2mm/min; ASTM D790 |
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® ECO BV 30 H2 900500 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Flexural Modulus | 8.87 GPa | 1290 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP IFP36 PA6.12 LNP* LUBRICOMP* IFP36 is a Nylon 6/12 base resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of t his grade include: Wear Resistant. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240U PP SABIC® PPcompound G3240U is a general purpose, 40% glass filled, chemically coupled, heat stabilized and UV stabilized homopolymer polypropylene compound. The IMDS ID is 209768078. |
|||
Flexural Modulus | 8.92 GPa | 1290 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 LNP* LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Flexural Modulus | 8.91 GPa | 1290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Flexural Modulus | 8.89 GPa | 1290 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF30 HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedProcessin.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 (Asia Pacific) LNP* Thermocomp* QF007 is a compound based on Nylon 6/10 resin containing Glass Fiber. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WX93111 PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* WX93111 is a compound based on Polybutylene Terephalate resin containing Flame retardant , Glass Fiber, Proprietary filler. Added features include : Improved CTI. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Asia Pacific) LNP* Thermocomp* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp ZF-1006 BK8-950 PPE+PS LNP* Thermocomp* ZF-1006 BK8-950 is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66 LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Flexural Modulus | 8.91 GPa | 1290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Toyobo VYLOPET® EMC317A Injection Molding Polyester Resin, Warpageless Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessInformation provided by Toyobo. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Plenco 4504 Phenolic, Granular, Injection Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790, ISO 178 |
EPICHEM Epinyl PA 66 GF 30 H Polyamide 66, 30% Glass, Heat Stabilized Characteristics: 30% glass fibre filled |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790, ISO 178 |
EPICHEM Epinyl PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
BLUESTAR 203G30 PBT, 30% Glass Filled Typical Applications: Thinner wall partsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Resinoid 7201 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |