Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.5 GPa | 2100 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 60 Polyamide 6, 60% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 60% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Niche Polymer PA66GF50BK Nylon 66, 50% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
PolyOne Nymax™ GF 1200 A 55 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | |
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6,6 GF50 HS L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO 178 |
Polyram Polytron P60B04-S Polypropylene, 60% Long Glass Fiber A chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Asahi Kasei Thermylon® NSG-440A-H 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | Tangent; ASTM D790 |
Applied Composites 8061 Polyester SMC Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Structural Grade Chopped Fibers, High Stiffness, High Fiber LoadingsInformation provided by Applied Composites Corp.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 433 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Asahi Kasei Thermylon® NSG-730A 65% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |