Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 14.5 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.41 - 14.5 GPa
350 - 2100 ksi
Average value: 4.72 GPa Grade Count:21
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
Flexural Modulus 10.5 - 14.5 GPa
1520 - 2100 ksi
Average value: 11.9 GPa Grade Count:12
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Flexural Modulus 11.7 - 14.5 GPa
1700 - 2100 ksi
Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade
BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, ..
Flexural Modulus 11.7 - 14.5 GPa
1700 - 2100 ksi
Bulk Molding Compounds BMC 1100 Corelyn Glass Fiber Reinforced Polyester Compound
BMC 1100, also known as CoreLyn, is a food contact safe material with excellent scratch and stain resistant properties. CoreLyn can be pigmented to match virtually any color. This glass fiber-reinfo..
Flexural Modulus 12.4 - 14.5 GPa
1800 - 2100 ksi
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade
BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B..
Flexural Modulus 7.52 - 14.5 GPa
1090 - 2100 ksi
Average value: 10.7 GPa Grade Count:10
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..