Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.00 GPa | 145 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE D 6208 BLK Ash is 2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
NYCOA 2084 HS PA 6 lubricated flexible tubing and conduitInformation provided by NYCOA, Inc. |
|||
Flexural Modulus | >= 1.00 GPa | >= 145 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 6748F (486H6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers SEQUEL® 1514 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1514 engineered polyolefin material is designed to provide significantly greater mar resistance than conventional TPOs. SEQUEL® 1514 polyolefin is designed for automotive app.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
SABIC B5429/B5429A High Density Polyethylene for Blow Molding Product Description: B5429 Series grades are medium molecular weight High Density Polyethylene copolymer. They are primarily intended for blow molding articles of small sizes. B5429 series grades.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2709 HDPE Injection Molding Resin Features: Excellent cold temperature toughness, high stiffness.Applications: Housewares, containers, pails, closures.Data provided by the manufacturer. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 1% secant; ASTM D790A |
Reliance Industries Repol B120MA Polypropylene REPOL Polypropylene B120MA is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 8623 Polypropylene Impact Copolymer Key Features: super-high impact polypropylene copolymer resin, good stiffness, FDA acceptableApplications: automotive parts, luggage, totes, bins, carrying cases, appliancesMeets FDA requirements in.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
Flint Hills 23M2A Polypropylene Random Copolymer Features: High contact clarity, blush resistant, good impact, and stress resistant, good auto-clave stability, and low extractability. Product does not contain animal derived components.Application.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66 PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ ETA-4161UV Thermoplastic Olefin Resin Key Features: fractional melt flow, medium high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good melt strength, excellent weatherabili.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ISO 178 |
Styrolution Styrolux T SBC Styrolux T is a new developmental, clear and tough styrene-butadiene copolymer (SBC) designed specifically for high performance film extrusion and shrink film applications. Styrolux T has been devel.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5502 GA HDPE Blow Molding Applications:Blow molded containers up to 30 liters for packagingChemicalsHousehold productsOils and foodstuffsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemi.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H1000PC High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, low sagging, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 5 mm/min, secant; ASTM D790 |
A. Schulman PP 1407L-01 Polypropylene High-Impact Copolymer Polypropylene DescriptionPolypropylene PP 1407L-01 is a super high-impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 1500X-01 Polypropylene High Impact Copolymer Polypropylene DescriptionPolypropylene PP 1500X-01 is a specially formulated high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 - 1.14 GPa | 145 - 165 ksi | tangent; ASTM D790 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 - 1.14 GPa | 145 - 165 ksi | tangent; ASTM D790 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 1692 Polypropylene High Impact Copolymer DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2550A Thin Walled Injection Molding Polypropylene Medium Impact CopolymerApplications: Housewares, containers and other rigid packaging.Formolene 2550A is a medium impact, high flow, controlled rheology copolymer of polypropylene designed for such .. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
Aclo Accucomp Polypropylene CPO406L Copolymer |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437C30L1 Calcium Reinforced |
|||
Flexural Modulus | >= 1.00 GPa | >= 145 ksi | ISO 178 |
AKG Polymers Vision PP PPC TC3005 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | Injection Molded; ISO 178 |
Braskem INSPIRE™ 137 NA Performance Polypropylene Polymer INSPIRE™ 137 Performance polymer is an impact copolymer, primarily designed for film extrusion and suitable for blow molding where high mechanical properties are of the highest importance.INSPIRE 1.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ISO 178-2 |
Total Lacqtene® 2001 TN 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TN 46 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2001 TN 46 is used for sewage pipe, smooth protective condu.. |