Mechanical Properties Metric English Comments
Flexural Modulus 10.95 GPa
1588 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Branched (Asia Pacific)
LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 10.95 GPa
1588 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched
LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Flexural Modulus 10.95 GPa
1588 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched (Europe-Africa-Middle East)
LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 10.95 GPa
1588 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS (Asia Pacific)
LNP* Lubricomp* OFL36A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.