Polymer Property : Flexural Modulus = 1659 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 11.44 GPa
1659 ksi
ASTM D790
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East)
LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Flexural Modulus 11.44 GPa
1659 ksi
ASTM D790
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66
LNP* KONDUIT* RTF2B is a compound based on Nylon 66 resin containing 10% Glass Fiber, 55% Thermal Filler. Added features of this material include: Thermally Conductive.
Flexural Modulus 11.44 GPa
1659 ksi
ASTM D790
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific)
LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Flexural Modulus 11.44 GPa
1659 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp OFP36A PPS - Branched
LNP LUBRICOMP* OFP36A is a compound based on PPS - Branched resin containing Glass Fiber, Silicone, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SA..
Flexural Modulus 11.44 GPa
1659 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp OFP36A PPS - Branched (Asia Pacific)
LNP LUBRICOMP* OFP36A is a compound based on PPS - Branched resin containing Silicone, PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.This data was supplied by SA..
Flexural Modulus 11.44 GPa
1659 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OX88533 PPS
LNP LUBRICOMP* OX88533 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Flexural Modulus 11.44 GPa
1659 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66
LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 11.44 GPa
1659 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA6.10
LNP* THERMOCOMP* QF00A is a compound based on Nylon 6/10 containing 50% Glass Fiber.