Mechanical Properties Metric English Comments
Flexural Modulus 2.90 - 11.7 GPa
420 - 1700 ksi
Average value: 9.21 GPa Grade Count:5
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va..
Flexural Modulus 3.44 - 11.7 GPa
499 - 1700 ksi
Average value: 6.04 GPa Grade Count:23
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Flexural Modulus 3.38 - 11.7 GPa
490 - 1700 ksi
Average value: 5.50 GPa Grade Count:4
Overview of materials for Polyphenylene Ether, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu..
Flexural Modulus 5.66 - 11.7 GPa
821 - 1700 ksi
Average value: 7.58 GPa Grade Count:4
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Flexural Modulus 0.965 - 11.7 GPa
140 - 1700 ksi
Average value: 4.13 GPa Grade Count:61
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Flexural Modulus 8.07 - 11.7 GPa
1170 - 1700 ksi
Average value: 10.2 GPa Grade Count:3
Overview of materials for Phenolic, Graphite Cloth Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Graphite Cloth Composite". Each property range of values reported is minimum and maximum value..
Flexural Modulus 2.10 - 11.7 GPa
305 - 1700 ksi
Average value: 6.03 GPa Grade Count:78
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Flexural Modulus 3.10 - 11.7 GPa
450 - 1700 ksi
Average value: 7.93 GPa Grade Count:4
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Flexural Modulus 11.0 - 11.7 GPa
1600 - 1700 ksi
ASTM D790
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Flexural Modulus 11.0 - 11.7 GPa
1600 - 1700 ksi
ASTM D790
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Flexural Modulus 10.3 - 11.7 GPa
1500 - 1700 ksi
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound
BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
Flexural Modulus 10.3 - 11.7 GPa
1500 - 1700 ksi
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound
BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty..
Flexural Modulus 7.00 - 11.7 GPa
1020 - 1700 ksi
Average value: 9.72 GPa Grade Count:39
Overview of materials for Polycarbonate, 40% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E..
Flexural Modulus 6.90 - 11.7 GPa
1000 - 1700 ksi
Average value: 10.3 GPa Grade Count:8
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma..
Flexural Modulus 3.40 - 11.7 GPa
493 - 1700 ksi
Average value: 7.81 GPa Grade Count:22
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Flexural Modulus 10.3 - 11.7 GPa
1500 - 1700 ksi
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound
BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression..
Copyright © lookpolymers.com All Rights Reserved