Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.3 GPa | 1780 ksi | X, Y direction; Condition A; ASTM D790 |
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Flexural Modulus | 12.3 GPa @Temperature 23.0 °C |
1780 ksi @Temperature 73.4 °F |
ISO 178 |
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Flexural Modulus | 12.3 GPa @Temperature 23.0 °C |
1780 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D201 FB52 PBT, Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN133G50 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66 LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RE004 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing Glass Fiber. Added features include: Easy Molding. |
|||
Flexural Modulus | 12.27 GPa | 1780 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF PF00AIS PA 6 (Asia Pacific) LNP* THERMOTUF* PF00AIS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 226F10 Nylon 6.6, 50% Glass Fiber SAXAMID 226F10 is a polyamide 6.6 injection-molding-grade reinforced with 50% glass fibers. It has high mechanical strength.Information provided by SAX Polymers |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Europe-Africa-Middle East) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | ASTM D790 |
Plenco 08122 Polyester BMC, Compression Molded PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60G8 Nylon 66, 40% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |
|||
Flexural Modulus | 12.3 GPa | 1780 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON ME006 PP LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 12.27 GPa | 1780 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF PF00AIS PA 6 LNP THERMOTUF* PF00AIS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |